Yes,, optimizing the cooling rate is vital. Rapid cooling can cause thermal stresses that lead to cracks, especially in larger pieces like a 32 quart pot. We use a controlled cooling process to avoid this. Additionally, make sure the foundry has experience with large-scale castings. Some foundries in China specialize in smaller parts and might not have the right equipment for something this size.